Sunday, 1 April 2018

Entering light fabrication (Stainless steel)










Before i go to Poland for working as a welder in light fabrication industry (Konstal Sp.o.o) i got this great opportunity to exercise my skill in it especially in thin material 3mm-1,4 mm stainless steel. i met great people and mentor in this local company that is i believe this company will be Big in sort coming years.

welded using pulse TIG in 14ga stainless steel.
Full amperage and running without wire.

a note for remainder :

stainless is hate heat so running "below radar" or control your heat to keep your workpiece still in form.





















 